Pametne prevleke za zaščito konstrukcijskih materialov
Anja Copot, 2020, undergraduate thesis

Abstract: Korozija povzroča degradacijo kovinskih materialov, ki so v stiku s tekočino ali plinom. Sam proces se pospeši z izpostavitvijo visokim temperaturam, kislinam in solem. Posledično se spremenijo lastnosti materiala in nastaja škoda pri samem tehnološkem procesu. Da bi korozijo upočasnili, uporabljamo različna inhibitorna sredstva, ki so lahko organske ali anorganske narave. Diplomsko delo prikazuje študijo pametnih prevlek kot zaščito pred korozijskimi procesi na kovinski površini. Prevleka vsebuje inkapsuliran inhibitor, ki se sprosti, ko se nahaja v agresivnem okolju. Njegovo delovanje lahko zapolni poškodbe na prevleki, ki nastanejo ob fizični poškodbi, ob spremembi pH na medfazni površini med prevleko in korozivnim medijem ter podobnim. Ovojnica kapsule se ob tem predre, sprošča se inhibitor, ki se običajno adsorbira na površino in na tak način nudi dodatno zaščito pred korozijo. Uporabili smo vzorce iz aluminijeve zlitine tipa EN AW 6451 in jih predhodno obdelali tako, da je bila oprijemljivost prevleke iz epoksidne smole z inkapsuliranimi delci inhibitorja čim večja. Zaščitni sloj smo nanesli z metodo 'spin coatinga', ki ustvari enakomerno tanek sloj zaščitne prevleke na površini preiskovanega vzorca. Testirane prevleke so vsebovale tri različne koncentracije inkapsuliranih delcev inhibitorja. Največjo inhibicijsko učinkovitost je imela 'pametna prevleka' z najvišjim utežnim odstotkom inkapsuliranih delcev, ki so vsebovali kationski surfaktant. Za korozivni medij smo uporabili vodno raztopino natrijevega klorida z dvema različnima koncentracijama (3,5 % in 0,1 mol/L). Meritve smo izvedli na vzorcih po 30-minutni stabilizaciji v raztopini na mirovnem potencialu in po 48 urni predhodni izpostavitvi korozivnemu okolju. V posameznih primerih smo dosegli tudi najvišjo možno vrednost inhibicijske učinkovitosti in sicer  = 99 % - 100 % .
Keywords: korozija, protikorozijska zaščita, pametne prevleke, inhibicijska učinkovitost, inkapsuliran inhibitor
Published: 08.10.2020; Views: 166; Downloads: 46
.pdf Full text (1,69 MB)

2.
Kofein kot inhibitor korozijskih procesov v agresivnem mediju
Klara Laura Konda, 2020, undergraduate thesis

Abstract: V diplomskem delu je predstavljen kofein kot zeleni inhibitor korozije. Zeleni inhibitorji korozije ali t. i. okolju prijazni inhibitorji korozije so netoksične spojine, ki imajo sposobnost upočasnjevati degradacijo kovin v procesu korozije. Vpliv kofeina na inhibicijo korozije smo preučevali na vzorcih nerjavnega avstenitnega jekla z oznako AISI 304/W.Nr.1.4301, ki so bili izpostavljeni korozijskemu okolju raztopin HCl in H2SO4 različnih koncentracij za različna časovna obdobja (štiri, osem in 24 ur). Pri eksperimentalnem delu smo na vzorcih nerjavnega avstenitnega jekla uporabili naslednje metode: brušenje z vodo brusnim papirjem različnih granulacij, ultrazvočno čiščenje, metodo gravimetrije, mikroskopiranje in analizo z infrardečo spektroskopijo s Fourierjevo transformacijo na oslabljeni totalni odboj (ATR-FTIR). Ugotovljeno je bilo, da 8,5 % raztopina HCl predstavlja ustrezen, še dovolj agresiven medij. V slednjem smo analizirali inhibicijsko učinkovitost kofeina ƞ (%) ob dodatku 1 %, 2 %, 5 % in 10 % masnega deleža kofeina (wk). Izračunali smo korozijsko hitrost r (mm/leto) brez dodanega inhibitorja in z dodanim inhibitorjem. V 8,5 % raztopini HCl smo dosegli najnižjo inhibicijsko učinkovitost kofeina 36,3 % z 1 % dodanega kofeina v času štirih ur in najvišjo inhibicijsko učinkovitost kofeina 69,2 %, z 10 % dodanega kofeina v času osmih ur. Korozijska hitrost v 8,5 % raztopini HCl v primeru dodanega inhibitorja je najvišja pri 1 % dodanega kofeina in znaša 0,80 mm/leto ter najnižja pri 10 % dodanega kofeina in znaša 0,42 mm/leto. Obe hitrosti sta pridobljeni v času osmih ur. Osem ur tako predstavlja prelomen čas, medtem ko 5 % dodanega kofeina predstavlja mejno koncentracijo dodanega inhibitorja.
Keywords: kofein, inhibitor, korozija, agresivni medij, nerjavno jeklo
Published: 08.10.2020; Views: 148; Downloads: 31
.pdf Full text (2,06 MB)

3.
Inhibicijska učinkovitost propolisa v namen zaščite konstrukcijskih materialov
Simona Sedonja, 2020, undergraduate thesis

Abstract: S klasično elektrokemijsko potenciodinamsko metodo smo proučevali inhibitorni vpliv treh naravnih produktov, dostopnih v široki potrošnji, na bakru v kislem mediju. Izbrali smo t. i. »čebelje produkte« v treh različicah in sicer: propolis, matični mleček in apisirup. V primeru propolisa smo baker predhodno zaščitili s plastjo, ki je nastala po potopitvi vzorca v etanolno raztopino stearinske kisline ob dodatku različnih koncentracij propolisa (c = 0,5-%, 1,0-%, 2,0-% ter 4,0-%). S tem smo dosegli hidrofoben karakter modificirane površine bakra, kar se je pokazalo kot rezultat z najvišjo vrednostjo inhibicijske učinkovitosti η = 93-99 %. Hidrofobna površina namreč otežuje neposreden kontakt z vodnimi raztopinami, kar simulirana raztopina kislega dežja nedvomno tudi je. Matični mleček in apisirup pa sta bila v procesu eksperimenta neposredno dodana v korozivni medij. Dosežena vrednost inhibicijske učinkovitosti je bila v tem primeru nekoliko nižja η = 80-97 %, kar pripisujemo tekmovalnemu odnosu med procesom adsorpcije in desorpcije inhibitorja na površino bakra. Desorpcija je nedvomno povzročena s korozijskimi reakcijami oz. je odvisna od hitrosti le-teh. Na osnovi dobljenih rezultatov lahko zatrdimo, da so vsi trije inhibitorji za izbran korozijski sistem dosegli visoko stopnjo inhibicije, kar jih uvršča med potencialne inhibitorje korozijskih procesov.
Keywords: korozija, inhibitor, propolis, potenciodinamska metoda, inhibicijska učinkovitost
Published: 08.10.2020; Views: 147; Downloads: 31
.pdf Full text (2,67 MB)

4.
Electrochemical and surface analysis of 2-phenylimidazole adsorbed on copper from chloride solution
Matjaž Finšgar, Klodian Xhanari, 2018, original scientific article

Abstract: The electroanalytical and surface characterization of copper immersed in 3 wt.% NaCl solution containing 1 mM of 2-phenylimidazole (2PhI) is presented. It was proven that 2PhI can be employed as corrosion inhibitor for copper using various electrochemical analyses, such as cyclic voltammetry, chronopotentiometry, electrochemical impedance spectroscopy, and potentiodynamic curve measurements. The adsorption of 2PhI on copper was further analyzed by 3D-profilometry, attenuated total reflectance Fourier transform infrared spectroscopy, contact angle measurements, and scanning electron microscopy equipped with an energy dispersive X-ray spectrometer. This system was therefore comprehensively described by various analytical approaches.
Keywords: corrosion inhibitor, copper, electrochemical impedance spectroscopy, EIS, cyclic voltammetry, attenuated total reflectance Fourier transform infrared, ATR-FTIR
Published: 17.01.2019; Views: 826; Downloads: 269
.pdf Full text (5,88 MB)
This document has many files! More...

5.
The influence of $Ce^{3+}$ ions on the corrosion rate of stainless steel in acidic solutions of different pH-values
Aljana Petek, Sebastijan Kovačič, 2014, original scientific article

Abstract: The corrosion resistance of AISI 420 stainless steel in 0.1 mol $L^{−1}$ $H_2SO_4$ + 0.1 mol $L^{−1}$ $Na_2SO_4$ solutions at different pH-values and the inhibiting effect of $Ce^{3+}$ ions was studied using electrochemical polarization methods. The results reveal decreasing of the corrosion rate with an increasing the pH of the solution, which demonstrates the progressive protective character of the inhibitor used. At pH lower than 3.33, the corrosion inhibition was most probably a result of the competitive adsorption of $Ce^{3+}$ with $H^+$ ions on the cathodic sites of the electrode surface, and it was found to be dependent on the relative concentration of $H^+$/$Ce^{3+}$. The peroxide generated from the oxygen reduction reaction at pH 3.33 was found to be capable oxidize trivalent cerium (Ce) to the tetravalent state. As obtained hydroxide precipitates act as diffusion barrier hindering the corrosion processes, whereafter a spontaneous passivity occurs on the steel surface at this pH.
Keywords: acid corrosion, green corrosion inhibitor, stainless steel, electrochemical techniques
Published: 24.07.2017; Views: 644; Downloads: 263
.pdf Full text (463,32 KB)
This document has many files! More...

6.
Urokinase plasminogen activator (uPA) and plasminogen activator inhibitor type-1 (PAI-1) in breast cancer
Maja Lampelj, Darja Arko, Nina Čas-Sikošek, Rajko Kavalar, Maja Ravnik, Barbara Jezeršek Novaković, Sarah Dobnik, Nina Fokter Dovnik, Iztok Takač, 2015, original scientific article

Abstract: Background: Urokinase plasminogen activator (uPA) and plasminogen activator inhibitor type-1 (PAI-1) play a key role in tumour invasion and metastasis. High levels of both proteolytic enzymes are associated with poor prognosis in breast cancer patients. The purpose of this study was to evaluate the correlation between traditional prognostic factors and uPA and PAI-1 expression in primary tumour of breast cancer patients. Patients and methods: 606 primary breast cancer patients were enrolled in the prospective study in the Department of gynaecological oncology and breast oncology at the University Medical Centre Maribor between the years 2004 and 2010. We evaluated the traditional prognostic factors (age, menopausal status, tumour size, pathohistological type, histologic grade, lymph node status, lymphovascular invasion and hormone receptor status), together with uPA and PAI-1. We used Spearman%s rank correlation, Mann Whitney U test and X2 test for statistical analysis. Results: Our findings indicate a positive correlation between uPA and tumour size (p < 0.001), grade (p < 0.001), histological type (p < 0.001), lymphovascular invasion (p = 0.01) and a negative correlation between uPA and hormone receptor status (p < 0.001). They also indicate a positive correlation between PAI-1 and tumour size (p = 0.004), grade (p < 0.001), pathohistological type (p < 0.001) and negative correlation between PAI-1 and hormone receptor status (p = 0.002). Conclusions: Our study showed a relationship between uPA and PAI-1 and traditional prognostic factors. Their role as prognostic and predictive factors remains to be further evaluated.
Keywords: urokinase plasminogen activator, plasminogen activator inhibitor, breast cancer
Published: 05.04.2017; Views: 622; Downloads: 67
.pdf Full text (597,75 KB)
This document has many files! More...

7.
Napovedna moč nekaterih kliničnih, histopatoloških in bioloških parametrov za preživetje bolnic z rakom dojk brez zasevkov v bezgavkah, zdravljenih v Univerzitetnem kliničnem centru Maribor v letih 2000–2009
Nina Fokter Dovnik, 2017, doctoral dissertation

Abstract: Izhodišča. Enega izmed največjih izzivov pri zdravljenju raka dojk v zgodnjem stadiju predstavlja izbor bolnic s predvidenim agresivnejšim potekom bolezni, ki potrebujejo dopolnilno sistemsko zdravljenje. O tem se odločamo na podlagi različnih napovednih dejavnikov, kot so status pazdušnih bezgavk, velikost tumorja, stopnja diferenciacije, limfovaskularna invazija, starost bolnic, status hormonskih receptorjev, status HER2, v zadnjem času pa v ta namen ponekod uporabljajo tudi urokinazni aktivator plazminogena (uPA) in inhibitor aktivatorja plazminogena 1 (PAI-1). Vloga novejših napovednih dejavnikov v primerjavi s tradicionalnimi še ni povsem razjasnjena. Namen raziskave je bil ugotoviti vpliv posameznih dejavnikov na preživetje bolnic z rakom dojk brez zasevkov v bezgavkah, zdravljenih v Univerzitetnem kliničnem centru (UKC) Maribor. Hkrati sem želela tudi primerjati preživetje bolnic, zdravljenih v UKC Maribor, s slovenskim povprečjem. Bolnice in metode. Opravila sem retrospektivno analizo bolnic z invazivnim rakom dojk brez zasevkov v bezgavkah, ki so bile primarno zdravljene v UKC Maribor v letih 2000–2009. Podatke sem pridobila iz medicinske dokumentacije in jih dopolnila s podatki iz Registra raka Republike Slovenije, od koder sem pridobila tudi podatke o vseh primerljivih slovenskih bolnicah, zdravljenih v istem obdobju. Analizirala sem korelacije med napovednimi dejavniki in s pomočjo Coxove regresije in Coxovega modela sorazmernih tveganj opravila univariatne in multivariatne analize preživetja brez bolezni, celokupnega in specifičnega preživetja. Rezultati. Študijsko skupino je sestavljalo 858 bolnic s srednjim časom sledenja 101 mesec. Med bolnicami, zdravljenimi v UKC Maribor, in vsemi slovenskimi bolnicami ni bilo razlik v celokupnem (HR 1,07; 95 % CI 0,91–1,27; p = 0,413) in specifičnem preživetju (HR 0,85; 95 % CI 0,66–1,11; p = 0,234). Preživetje brez bolezni (HR 0,67; 95 % CI 0,50–0,91; p = 0,010) in specifično preživetje (HR 0,53; 95 % CI 0,30–0,94; p = 0,031) je bilo statistično značilno boljše v obdobju 2005–2009 v primerjavi z 2000–2004, pri celokupnem preživetju pa se je kazal enako usmerjen statistično neznačilen trend (HR 0,73; 95 % CI 0,51–1,05; p = 0,087). Med napovednimi dejavniki so bile prisotne številne korelacije. V multivariatnih analizah so na preživetje brez bolezni najbolj vplivali starost ob diagnozi, vrednost uPA/PAI-1 in status estrogenskih receptorjev, na celokupno preživetje starost, stopnja diferenciacije in vrednost uPA/PAI-1, na specifično preživetje pa stopnja diferenciacije. Zaključki. Preživetje bolnic z rakom dojk brez zasevkov v bezgavkah, primarno zdravljenih v UKC Maribor v letih 2000–2009, je zelo visoko in enakovredno preživetju vseh primerljivih bolnic na ravni Slovenije. Kot najpomembnejša napovedna dejavnika sta se pri tej skupini bolnic izkazala vrednost uPA/PAI-1 in stopnja diferenciacije, ki sta klinično pomembno vplivala na preživetje brez bolezni, celokupno in specifično preživetje.
Keywords: rak dojk brez zasevkov v bezgavkah, dopolnilno zdravljenje, stadij, stopnja diferenciacije, status HER2, status hormonskih receptorjev, urokinazni aktivator plazminogena, inhibitor aktivatorja plazminogena 1
Published: 14.03.2017; Views: 1019; Downloads: 132
.pdf Full text (5,97 MB)

8.
9.
VITAMIN C KOT INHIBITOR KOROZIJSKIH PROCESOV V KISLEM MEDIJU
Tanja Kondić, 2012, undergraduate thesis

Abstract: V diplomskem delu smo proučevali korozijsko obnašanje nerjavnega jekla PROKRON 1 v različnih koncentracijah HCl (c = 0,01; 0,1; 1,0 M HCl), ter ob različnih dodatkih inhibitorja (c = 0,0005; 0,001; 0,005; 0,01 M). Pri eksperimentalnem delu smo uporabili samo eno vrsto inhibitorja, in sicer vitamin C. Meritve so bile opravljene s potenciodinamsko polarizacijsko metodo, kjer smo primerjali inhibitorni učinek izbranega inhibitorja v prisotnosti različnih koncentracij vitamina C in HCl. V zaključnem delu meritev je bilo ugotovljeno, da se vitamin C obnaša z dvojnim delovanjem, saj ponekod deluje kot inhibitor, ponekod pa kot aktivator.
Keywords: nerjavno jeklo, korozija, inhibitor, vitamin C, klorovodikova kislina
Published: 16.10.2012; Views: 1478; Downloads: 196
.pdf Full text (2,64 MB)

10.
Effects of surfactants and their mixtures on inhibition of the corrosion process of ferritic stainless steel
Regina Fuchs-Godec, 2009, original scientific article

Abstract: The corrosion inhibition characteristics regarding mixtures of cationic/zwitterionic types of surfactant (Myristyltrimethylammonium bromide/Palmitylsulfo-betaineas), and non-ionic surfactant TRITON-X-405 mixed with 1 mM of KBr, as corrosion inhibitors for stainless steel (SS) (type X4Cr13) in aqueous solutions of 2 M H2SO4 were investigated using potentiodynamic polarisation measurements. The polarisation data showed that mixtures of the surfactants used in this study acted as mixed-type inhibitors, adsorbing on the stainless steel surface in agreement with the Flory-Huggins adsorption isotherm. The tensiometric results of this study suggest the existence of a second state of aggregation for zwitterionic/cationic surfactant mixtures. From these values of the free energy of adsorption, which in both mixtures decreased with respect to a single surfactant, we concluded that the adsorption in mixtures was stronger. The mixtures studied here showed good inhibition properties for ferritic stainless steel type X4Cr13 in 2 M H2SO4 solution.
Keywords: corrosion inhibitor, cationic surfactant, Zwitterionic surfactant, Flory-Huggins isotherm, Sulphuric acid
Published: 01.06.2012; Views: 1120; Downloads: 100
URL Link to full text

Search done in 0.17 sec.
Back to top
Logos of partners University of Maribor University of Ljubljana University of Primorska University of Nova Gorica